Wearing of NiP electrolytic coatings at sliding friction
UDC
УДК 629.7.023.222:620.178.162
DOI
10.18577/2307-6046-2015-0-3-8-8
Article PDF (Russian)
(742.95 KB)
How to cite
Aslanyan I.R., Schuster L.S. Wearing of NiP electrolytic coatings at sliding friction // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-8-8. URL: https://test.viam.ru/en/journal/2015/3/8
Abstract
An effect of reinforcing silicon carbide additives and heat treatment on the wear of nickel-phosphorous coatings (NiP) produced by electrodeposition was investigated. It was found that the wear of the investigated coatings could have an abrasive-oxidative nature: predominantly abrasive for NiP–SiC composite coatings and predominantly oxidative for NiP coatings accompanied by fatigue fracture of nickel oxides. Additives of SiC allow increasing the hardness of electrolytic coatings, but they prevent fixation of oxide films formed during friction on the contact surface. Heat treatment increases the hardness of the coatings due to deposition of the crystalline phase Ni3P, which reduces the wear rate of the coatings.
Reference list
- Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Pomelov Ja.A. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protective coatings for gas turbine engine blades] //Konversija v mashinostroe-nii. 1999. №2. S. 42–47.
- Litye lopatki gazoturbinnyh dvigatelej. Splavy, tehnologii, pokrytija [Alloy blades of gas turbine engines. Alloys Technology, coating]. 2-e izd. /Pod obshh. red. E.N. Kablova. M.: Nauka. 2006. 632 s.
- Kablov E.N., Muboyadzhyan S.A. Heat-resistant coatings for the high-pressure turbine blades of promising GTES //Russian metallurgy (Metally). 2012. V. 2012. №1. P. 1–7.
- Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S. Nanoslojnye uprochnjajushhie pokrytija dlja zashhity stal'nyh i titanovyh lopatok kompressora GTD [Nanolayer strengthening coatings for protection of steel and titanium compressor blades of GTE] //Aviacionnye materialy i tehnologii. 2011. №3. S. 3–8.
- Kablov E.N. Korrozija ili zhizn' [Corrosion or life] //Nauka i zhizn'. 2012. №11. S. 16–21.
- Mubojadzhjan S.A., Galojan A.G. Kompleksnye termodiffuzionnye zharostojkie pokrytija dlja bezuglerodistyh zharoprochnyh splavov na nikelevoj osnove [Integrated thermal diffu-sion heat-resistant coatings for carbon-free heat-resistant nickel-based alloys] //Aviacionnye materialy i tehnologii. 2012. №3. S. 25–30.
- Kablov E.N., Mubojadzhjan S.A. Teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Thermal barrier coatings for turbine blades of high-pressure turbine engine perspective] //Metally. 2012. №1. C. 5–13.
- Kablov E.N., Mubojadzhjan S.A. Zharostojkie i teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Heat-resistant and heat-resistant coatings for high-pressure turbine blades promising GTD] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnjajushhie ionno-plazmennye pokrytija dlja lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coatings for blades and other critical parts of the compressor GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
- Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protective coatings for gas turbine engine blades] //Metally. 2007. №5. S. 23–34.
- Semenychev V.V., Salahova R.K., Tjurikov E.V., Il'in V.A. Zashhitnye i funkcional'nye gal'vanicheskie pokrytija, poluchaemye s primeneniem nanorazmernyh chastic [Functional and protective electroplated coatings obtained using nanoscale particles] //Aviacionnye materialy i tehnologii. 2012. №S. S. 335–342.
- Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravlenija razvitija konstrukcionnyh materialov i tehnologij ih pererabotki dlja aviacionnyh dvigatelej nastojashhego i budushhego [Strategic directions of development of structural materials and their processing technology for aircraft engines present and future] //Avtomaticheskaja svarka. 2013. №10. S. 23–32.
- Kablov E.N., Mubojadzhjan S.A., Lucenko A.N. Nanostrukturnye ionno-plazmennye zashhitnye i uprochnjajushhie pokrytija dlja lopatok gazoturbinnyh dvigatelej [Nanostructured ion-plasma protective and strengthening coatings for gas turbine engine blades] //Voprosy materialovedenija. 2008. №2 (54). S. 175–187.
- Apachitei I., Duszczyk J. Autocatalytic nickel coatings on aluminium with improved abrasive wear resistance //Surface and Coatings Technology. 2000. V. 132. №1. P. 89–98.
- Mehta S.C., Smith D.A., Erb U. Study of grain growth in electrodeposited nanocrystalline nickel-1.2 wt.% phosphorus alloy //Materials Science and Engineering A. 1995. V. 204. №1–2. P. 227–232.
- Jena A.K., Chaturvedi M.C. Effect of heat treatment of NiP coatings //Phase Transformation in Materials, Prentice Hall, Englewood Cliffs. 1992. P. 103–105.
- Chen C.K., Feng H.M., Lin H.C., Hon M.H. The effect of heat treatment on the micro-structure of electroless Ni–P coatings containing SiC particles //Thin Solid Films. 2002. V. 416. №1–2. P. 31–37.
- Pribytkov G.A., Polev I.V. i dr. Struktura i abrazivnaja iznosostojkost' kompozitov tugoplavkij karbid – metallicheskaja matrica. Ch. 1 [Structure and abrasive wear resistance of the composites refractory carbide - metal matrix] //Fizicheskaja mezomehanika. 2004. №7. S. 419–422.
- Hrushhov M.M., Babichev M.A. Abrazivnoe iznashivanie [Abrasive wear]. M.: Nauka. 1970. 252 s.
- Aslanjan I.R., Shuster L.Sh. Iznashivanie gal'vanicheskih nikel'-fosfornyh pokrytij [Wear a galvanic nickel-phosphorus coatings] //Vestnik mashinostroenija. 2010. №12. S. 34–38.