Destruction of two-phase titanium alloys in sea water

Orlov M.R., Naprienko S.A.
Orlov M.R., Naprienko S.A. Destruction of two-phase titanium alloys in sea water // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-10-10. URL: https://test.viam.ru/en/journal/2017/1/10
Keywords
two-phase titanium alloys, corrosion cracking, delayed fracture under load, corrosive environment, sea water, stress intensity factor.
Abstract

Features of static and low-cyclic fatigue fracture of two-phase titanium alloys VT3-1, VT6, VBT8, VT9, VТ18U and VТ22 in sea water and air were investigated by scanning electron microscopy. Threshold values of stress intensity factors in the conditions of static and low-cyclic loading corresponding to the beginning of crack propagation were determined by the mechanism of corrosion cracking. Work is performed within implementation of «The strategic directions of development of materials and technologies of their processing for the period till 2030» [1]: – direction 2. «Fundamental oriented researches, qualification of materials, non-destructive testing»; – direction 18. «Environmental test for providing protection of materials, structures and complex technical systems against corrosion, aging and biodamages».

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. K 80-letiyu VIAM [To VIAM 80 anniversary] // Zavodskaya laboratoriya. Diagnostika materialov. 2012. T. 78. №5. S. 78–82.
  3. Erasov V.S., Yakovlev N.O., Nuzhnyj G.A. Kvalifikatsionnye ispytaniya i issledovaniya prochnosti aviatsionnyh materialov [Qualification tests and researches of durability of aviation materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
  4. Kablov E.N., Grinevich A.V., Erasov V.S. Harakteristiki prochnosti metallicheskih aviacionnyh materialov i ih raschetnye znacheniya [Characteristics of durability of metal aviation materials and their calculated values] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 370–379.
  5. Drozdovskij B.A., Prohodceva L.V., Novosilceva N.I. Treshhinostojkost titanovyh splavov [Crack firmness of titanium alloys]. M.: Metallurgiya, 1983. 192 s.
  6. Polyanskij V.M., Puchkov Yu.A., Orlov M.R., Naprienko S.A., Lavrov A.V. Vliyanie rastyagivayushhih napryazhenij na korrozionnuyu stojkost titanovogo splava VT22 v vodnom rastvore NaCl [Influence of pulling stresses on corrosion resistance of BT22 titanium alloy in NaCl aqueous solution] // Materialovedenie. 2016. №7. S. 13–19.
  7. Orlov M.R., Puchkov Yu.A., Naprienko S.A., Lavrov A.V. Issledovanie ekspluatacionnogo razrusheniya lopatki ventilyatora aviacionnogo gazoturbinnogo dvigatelya iz titanovogo splava VT3-1 [Research of operational destruction of blade of the fan of the aviation gas turbine engine from BT3-1 titanium alloy] // Titan. 2014. №4. S. 23–30.
  8. Orlov M.R., Naprienko S.A., Lavrov A.V. Fraktograficheskij analiz ekspluatacionnogo razrusheniya diska kompressora vysokogo davleniya iz splava VT18U [Research of operational destruction of blade of the fan of the aviation gas turbine engine from VT18U titanium alloy] // Titan. 2014. №2. S. 16–21.
  9. Orlov M.R., Naprienko S.A., Lavrov A.V. Issledovanie razrusheniya dvuhfaznyh titanovyh splavov v usloviyah vozdejstviya morskoj vody [Research of destruction of two-phase titanium alloys in the conditions of influence of sea water] // Sb. dokl. IV Vseros. konf. po ispytaniyam i issledovaniyam svojstv materialov «TestMat-2014». M.: VIAM, 2014. S. 9.
  10. Naprienko S.A., Zajcev D.V., Popov M.A., Zavodov A.V. Osobennosti razrusheniya titanovogo splava VT41 pri udarnom (dinamicheskom) nagruzhenii pri razlichnyh temperaturah [Features of destruction of VT41 titanium alloy in shock (dynamic) loading at different temperatures] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 60–68. DOI: 10.18577/2071-9140-2016-0-2-60-68.
  11. Prohodceva L.V., Naprienko S.A. Osobennosti razrusheniya titanovogo splava VT41 v razlichnom strukturnom sostoyanii pri staticheskom i dinamicheskom nagruzhenii [Features of destruction of BT41 titanium alloy in different structural condition at static and dynamic loading] // Deformaciya i razrushenie materialov. 2014. №2. S. 42–47.
  12. Prohodtseva L.V., Filonova E.V., Naprienko S.A., Moiseeva N.S. Issledovanie zakonomernostej razvitiya processov razrusheniya pri ciklicheskom nagruzhenii splava VT41 [Research of patterns of development of processes of destruction at cyclic loading of alloy VТ41] // Aviacionnye materialy i tehnologii. 2012. №S. S. 407–412.
  13. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  14. Kashapov O.S., Novak A.V., Nochovnaya N.A., Pavlova T.V. Sostoyanie, problemy i perspektivy sozdaniya zharoprochnyh titanovyh splavov dlya detalej GTD [Condition, problems and perspectives of creation of heat resisting titanium alloys for GTE details] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 02. Available at: http://www.viam-works.ru (accessed: May 18, 2016).
  15. Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Vliyanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlya lopatok KVD [Influence of modes of thermal processing on structure and property of heat resisting titanium alloy for KVD blades] // Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.