Cermets for plain bearings (review)

Burkovskaya N.P., Sevostyanov N.V.
Burkovskaya N.P., Sevostyanov N.V. Cermets for plain bearings (review) // Proceedings of VIAM. 2023. No. 3. DOI: 10.18577/2307-6046-2023-0-3-84-94. URL: https://test.viam.ru/en/journal/2023/3/8
Keywords
antifriction materials, cermet material, plain bearings, coefficient of friction, wear resistance, friction pair, tribological unit
Abstract

The compositions, properties, methods of manufacturing of cermet materials for plain bearings of transport vehicles and other equipment are considered. It is shown that iron, copper, cobalt and nickel or alloys based on them are mainly used as the matrix material of cermet bearings. Ceramic filler is selected to improve strength characteristics, increase wear resistance and load-bearing capacity. An increase in lubricating characteristics is provided by the introduction of solid lubricants into the composition of cermet materials: graphite, BN or sulfides, as well as polymers.

Reference list
  1. Onishchenko G.G., Kablov E.N., Ivanov V.V. Scientific and technological development of Russia in the context of achieving national goals: problems and solutions. Innovations, 2020, no. 6 (260), pp. 3–16.
  2. Method for manufacturing high-temperature composite antifriction material: pat. 2695854 Rus. Federation; filed 15.01.18; publ. 29.07.19.
  3. Copper-based alloy sliding-bearing material and preparation method thereof: pat. CN 103602849; filed 10.10.13; publ. 09.03.16.
  4. Burkovskaya N.P., Sevostyanov N.V., Bolsunovskaya T.A., Efimochkin I.Yu. Improvement of materials for sliding bearings of internal combustion engines (review). Trudy VIAM, 2020, no. 1, paper no. 08. Available at: http://www.viam-works.ru (accessed: June 08, 2022). DOI: 10.18577/2307-6046-2020-0-1-78-91.
  5. Sliding supports. Suspension and steering. Autocomponents: business, technology, service: multifunctional portal of the Max Media Group publishing house. Available at: https://a-kt.ru/articles/opory-skolzheniya (accessed: June 08, 2022).
  6. Sevostyanov N.V., Rozen A.E., Buznik V.M., Loginov O.N., Usatii S.G., Bolsunovskaya T.A. Copper-fluoroplastic conductive composite material obtained by explosive pressing. Trenie i iznos, 2020, vol. 41, no. 1, pp. 55–62.
  7. Adamenko N.A., Trykov Yu.P., Fetisov A.V. Polymer and metal-polymer materials obtained by explosive processing. Perspektivnye materialy, 2004, no. 3, pp. 63–68.
  8. Fedorchenko I.M., Pugina L.I. Composite sintered antifriction materials. Kyiv: Naukova Dumka, 1980, 404 p.
  9. Ultra-high molecular weight polyethylene (UHMWPE) – a material for extreme conditions. Available at: https://www.catalysis.ru/block/index.php?ID=3&SECTION_ID=1487 (дата обращения: 22.07.2022).
  10. Kablov E.N., Startsev V.O. Systematical analysis of the climatics influence on mechanical properties of the polymer composite materials based on domestic and foreign sources (review). Aviacionnye materialy i tehnologii, 2018, no. 2 (51), pp. 47–58. DOI: 10.18577/2071-9140-2018-0-2-47-58.
  11. Migunov V.P., Chatynyan L.A., Ivanov E.V. et al. Wear-resistant and antifriction materials for friction units. Aviation industry, 1982, no. 8, pp. 71–73.
  12. Self-lubrication sintered metal powder bearing with high tenacity and preparation method of self-lubrication sintered metal powder bearing: pat. CN 105420604A; filed 05.11.15; publ. 23.03.16.
  13. High-strength self-lubricating metal ceramic bearing and preparation method thereof: pat. CN 105369146A; filed 05.11.15; publ. 02.03.16.
  14. Metal ceramic bearing with good self-lubrication performance and preparation method of metal ceramic bearing: pat. CN 105369140A; filed 05.11.15; publ. 02.03.16.
  15. Self-lubricating metal ceramic bearing with high bending resisting strength and preparing method of self-lubricating metal ceramic bearing: pat. CN 105385967A; filed 05.11.15; publ. 09.03.16.
  16. Self-lubricating metal ceramic bearing good in abrasion resistance and preparing method of self-lubricating metal ceramic bearing: pat. CN 105385929A; filed 05.11.15; publ. 09.03.16.
  17. Self-lubrication sintered metal powder bearing with good abrasion resistance and preparation method of self-lubrication sintered metal powder bearing: pat. CN 105420602A; filed 05.11.15; publ. 23.03.16.
  18. Anti-cracking self-lubricating metal ceramic bearing and preparation method thereof: pat. CN 105369147A; filed 05.11.15; publ. 02.03.16.
  19. Alloy powder for forming hard phase and ferriferous mixed powder using the same, and manufacturing method for wear resistant sintered alloy and wear resistant sintered alloy: pat. US 7294167B2; filed 18.11.04; publ. 13.11.07.
  20. Wear resistant sintered member: pat. US 7575619B2; filed 24.03.06; publ. 18.08.09.
  21. Wear-resistant sintered contact material, wear-resistant sintered composite contact component and method of producing the same: pat. US 7282078B2; filed 09.01.05; publ. 16.10.07.
  22. Manufacture of self-lubricative sliding material: pat. JP 532989A; filed 12.01.89; publ. 20.07.90.
  23. Particle-dispersed copper alloy and method for producing the same: pat. JP 4314226B2; filed 13.09.05; publ. 12.08.09.
  24. Sintered bearing: pat. CN 107252888A; filed 23.07.13; publ. 17.10.17.
  25. Patrushev A.Yu., Farafonov D.P., Serov M.M. Tungsten-free hard alloys: manufacturing methods, structure and properties (review). Trudy VIAM, 2021, no. 11 (105), paper no. 07. Available at: http://www.viam-works.ru (accessed: June 08, 2022). DOI: 10.18577/2307-6046-2021-0-11-66-81.
  26. Trofimenko N.I., Efimochkin I.Yu., Dvoretskov R.M., Batienkov R.V. Obtaining fine-grained cemented carbide alloys of the WC–Co system (review). Trudy VIAM, 2020, no. 1 (85), paper no. 09. Available at: http://www.viam-works.ru (accessed: June 08, 2022). DOI: 10.18577 / 2307-6046-2020-0-1-92-100.
  27. Elagina O.Yu., Buklakov A.G., Yanka L.E.V. Development of a new composite material for the teeth of the armament of support-centering devices. Treniye i iznos, 2017, vol. 38, no. 2, pp. 151–157.
  28. Cobalt-based composite material that a kind of wear-resisting rotation axis carbide enhances and preparation method thereof: pat. CN 108149126A; filed 02.12.16; publ. 12.06.18.
  29. Method for preparing Ni cementing WC base cemented carbide: pat. CN 101397614B; filed 04.11.08; publ. 15.10.15.
  30. Novel WC–Fe–Ni hard alloy roll ring and preparation method thereof: pat. CN 104894452A; filed 03.07.15; publ. 12.09.17.
  31. WC–Fe–Ni–Co–Cr cemented carbide roll collar with low cost and high performance: pat. CN 106435322A; filed 02.11.16; publ. 04.09.19.
  32. WC–Co hard alloy with binding phase enhanced by Ni3Al and preparation method thereof: pat. CN 102383021A; filed 21.11.11; publ. 13.02.13.
  33. Kritsky V.Yu., Zubko A.I. Investigation of the possibility of using ceramic aircraft bearings of a new generation in the structures of rotor bearings for gas turbine engines. Dvigatel, 2013, no. 3, pp. 24–26.
  34. Balinova Yu.A., Grashchenkov D.V., Shavnev A.A., Babashov V.G., Chainikova A.S., Kurbatkina E.I., Bolshakova A.N. High-temperature heat-shielding, ceramic and metal-ceramic composite materials for a new generation of aircraft. Vestnik Kontserna VKO «Almaz-Antey», 2020, no. 2 (33), pp. 83–92. DOI: 10.38013/2542-0542-2020-2-83-92.
  35. Plain bearings. Automobile directory. Available at: https://press.ocenin.ru/podshipniki-skolzheniya/#Metallkeram_podsip (accessed: June 08, 2022).