Evaluation of nickel-cobalt coating adhesion to fiberglass and carbon fiber–reinforced plastic by scratching
A nickel coating was deposited on samples from structural composite materials such as fiberglass and carbon plastic in the galvanic bath by the electrodeposition method and then the surface was scratched by the hardness meter under various degree of loading. The morphology of the scratches channels is studied; their width and depth depending on the applied load are measured. The calculations of tensions heading to local destructions are conducted using Viver’s formula. It is established that nickel-cobalt coating has high strength of adhesion with both kinds of composite materials; no chippage or exfoliation is detected. Work is executed within the frames of the complex scientific direction 13.2. «Constructional PСM» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Kablov E.N., Karimova S.A., Semenova L.V. Korrozionnaya aktivnost ugleplastikov i zashhita metallicheskih silovyh konstrukcij v kontakte s ugleplastikom [Corrosion activity ugleplastikov and protection of metal load bearing structures in contact with the carbon plastics] // Korroziya: materialy, zashhita. 2011. №12. S. 1–7.
- Titareva A.S., Kirillov V.N., Startsev O.V. Povedenie materialov v elementah konstrukcij aviacionnoj tehniki, izgotovlennyh s primeneniem PKM i sistem LKP v usloviyah umerenno teplogo klimata [Behavior of materials in structural components of aeronautical engineering, manufactured using PCM and PC systems under conditions of temperate thermal climate] // Aviacionnye materialy i tehnologii. 2013. №S2.
- Semenychev V.V., Salahova R.K., Smirnova T.B. Ocenka tokov korrozii razlichnyh par materialov metodom pryamogo izmereniya [Assessment of currents of corrosion of different couples of materials method of direct measurement] // Praktika protivokorrozionnoj zashhity. 2015. №2 (76). S. 44–50.
- Semenychev V.V., Smirnova T.B. O vozmozhnosti ocenki poristosti pokrytij potenciostaticheskimi metodami [About possibility of assessment of porosity of coverings potentiostatic methods] // Aviacionnye materialy i tehnologii. 2009. №2. S. 7–10.
- Semenychev V.V., Koshelev V.N., Panarin A.V. Ekologicheski bezopasnyj tehnologicheskij process naneseniya zashhitnyh piroliticheskih alyuminievyh pokrytij bez navodorozhivaniya stal'noj podlozhki [Ecologically safe technological process of drawing protective pyrolitic aluminum coverings without hydrogen saturation of steel substrate] // Izvestiya Samarskogo nauchnogo centra RAN. 2008. T. 1. Specialnyj vypusk. S. 18–23.
- Biryuk V.I., Golovan V.I., Gunyaev G.M., Kryuchkov E.I. Primenenie kompozicionnyh materialov v koncevoj chasti kryla dlya snizheniya vesa kryla v celom [Application of composite materials in end part of wing for wing total weight reduction] // Trudy TsAGI. Ser.: Prochnost, kolebaniya, resurs aviacionnyh konstrukcij i sooruzhenij. 2002. Vyp. 2658. S. 44–49.
- Erasov V.S., Krylov V.D., Panin S.V., Goncharov A.A. Ispytaniya polimernogo kompozitsionnogo materiala na udar padayushhim gruzom [Drop-weight impact testing of polymer composite material] // Aviacionnye materialy i tehnologii. 2013. №3. S. 60–64.
- Borisova N.V., Artemenko A.A., Sladkov O.M. Issledovanie processov na granice razdela faz pri nanesenii metallicheskih pokrytij na ugleplastik [Research of processes on limit of the section of phases when drawing metallic coatings on carbon plastic] // Plasticheskie massy. 2009. №1. S. 7–9.
- Popova S.S. Metallizaciya ugleplastikov galvanicheskim sposobom [Metallization carbon plastics in the galvanic way] // Plasticheskie massy. 2007. №3. S. 27–29.
- Syrkin V.G. CVD-metod. Himicheskoe parofaznoe osazhdenie [CVD method. Chemical vapor-phase deposition]. M.: Nauka, 2000. 496 s.
- Elektrolit nikelirovaniya: pat. 2293803 Ros. Federaciya [Nickel plating electrolyte: pat. 2293803 Rus. Federation]; zayavl. 01.08.05; opubl. 20.02.2007 Byul. №5. 6 s.
- Elektrolit nikelirovaniya: pat. 2449063 Ros. Federaciya [Nickel plating electrolyte: pat. 2449063 Rus. Federation]; zayavl. 05.04.11; opubl. 27.04.12 Byul. №12. 7 s.
- Nagaeva L.V. Primenenie nanoporoshkov v elektrolitah nikelirovaniya, kak sposob polucheniya nikelevyh pokrytij, po svojstvam, ne ustupayushhim hromovym pokrytiyam [Application of nanopowders in nickel plating electrolytes, as way of receiving nickel coverings, on the properties which are not conceding to chrome plating] // Korroziya: materialy, zashhita. 2007. №9. S. 32–36.
- Salahova R.K., Semenychev V.V., Tyurikov E.V. Izbiratelnoe nanesenie zashhitnyh elektrohimicheskih pokrytij [Selective drawing protective electrochemical coatings] // Galvanotehnika i obrabotka poverhnosti. T. XVI. 2008. №4. S. 36–40.
- Naletov B.P., Sysoev E.K., Salahova R.K., Tyurikov E.V. Lokalnye metody naneseniya gal'vanicheskih pokrytij [Local methods of drawing galvanic coverings] // Izvestiya Samarskogo nauchnogo centra RAN. 2008. T. 1. Specialnyj vypusk. S. 33–37.
- P. Benjamin, C. Weaver. Measurement of Adhesion of Thin Films // Proc. Royal. Society. London. 1960. P. 163–176.
- Weaver C. Adhesion of Thin Films // Vac. Sci. Technol. 1975. P. 18–25.
- Mihajlin Yu.A. Konstrukcionnye polimernye kompozicionnye materialy [Constructional polymeric composite materials]. M.: Nauchnye osnovy i tehnologii, 2010. 558 s.
- Sinkevich Yu.V., Belyaev G.Ya., Yankovskij I.N. Vliyanie elektroimpulsnogo polirovaniya podlozhki na prochnost scepleniya galvanicheskih pokrytij [Influence of electropulse polishing of substrate on durability of coupling of galvanic coverings] // Progresivnі tehnologії і sistemi mashinobuduvannya. 2009. №1–37 (37). S. 228–232.